Are there any methods of "unyellowing" old beige PC parts?
Solution 1:
Have a look at the retr0bright page.
“The problem was finally cracked in late July 2008 with a mixture of hydrogen peroxide, a small amount of an “Oxy” laundry booster as a catalyst and a UV lamp; we believed that this could do the job in hours instead of days. "
Forum support thread on AmiBay.
After and before:
Solution 2:
Pencil eraser does this. It's a bit manual and takes a while (depending on the size of the eraser employed).
Using a pencil eraser, you can write frustrated messages to IT staff who have condemned you to labor on equipment old enough to still be beige/yellowed.
Solution 3:
I am re-posting the text content from Merlin, because websites die, and this tech should live and spread :) Original:
For those who don't know what we are on about, Retr0brite is a nickname that we coined for a process that can reverse yellowing of plastics.
Here's a catch-up on what has been discovered, this was taken from VCF and was written by yours truly. Props to AMike and Luzypher at a1k.org, rkauer, tonyyeb and others at EAB and the guys over at VCF for their help with the experiments; this has truly been a global effort and I am proud that it's in the public domain.
The original thread is over 200 posts long now and getting to be a heavy read for some, so Lorne and I thought it was best that we start a new thread here, with a "Story So Far" summary, before we start more experiments.
So, what has been discovered and learned so far?
We have learned that a magic concoction has been created that can reverse the years of yellowing of plastics, caused by the brominated flame retardants (which were added to the plastic when it was a masterbatch) migrating to the surface of the plastic and attracting oxygen molecules which become attached by a co-ordinate bond.
Bromine molecules are susceptible to ultra-violet light, in that chemical bonds involving bromine molecules can become destabilised if irradiated by UV light. This is what we are exploiting to remove the oxygen molecule from the brominated flame retardant.
The yellowing can be reversed to a degree by immersing parts in hydrogen peroxide or "Oxy" on their own, however, on their own they don't do that much; what is needed is a chemical called TAED (tetra acetyl ethylene diamine), which is a chemical found in the "Oxy" type laundry boosters. Why is this useful? It's useful because it catalyses perborates and percarbonates in the "Oxy" to produce peroxides; it can also catalyse hydrogen peroxide, which is exactly what we want. This is what makes the mixture much more potent.
The optimum mixture and conditions for reversing yellowing of plastics seems to be the following:-
A) Hydrogen peroxide solution, the strongest you can lay hands on; B) UV light, either as sunlight or a UV lamp; C) Approx 1/4 teaspoonful per gallon of "Oxy" laundry booster.
Parts immersed in this mixture will have the yellowing reversed in six to eight hours on average. Severe yellowing may take longer but it will only be a matter of a day or two. The mixture once made will last about four days before all of the peroxide is spent.
A more recent development is that the mixture can be made into a gel. Initial tests with Xanthan Gum added to the original mixture have shown that it can be made into a thicker material which can be brushed onto surfaces. This mixture foams up but still removes the yellowing when put under UV light, and can remove yellowing in four to six hours. This method also drastically cuts down on the amount of liquid required and means large areas can be treated at a relatively low cost. Other thickeners such as corn starch, hydroxy ethyl cellulose, wallpaper paste, latex or similar inert thickener may also work, however, tests are in the early stages, feel free to try some of these and report back if they work.
Recent tests by Lorne have shown that powdered hair bleach and hydrogen peroxide solution can give a similar effect to the original "Oxy" mixture, however, there may be side effects associated with using this material; early tests have seen adverse effects on paint and stickers may also be affected by this product. The original "Oxy" mixture does not affect paint or stickers, unless the stickers are held on with a water based glue or are paper stickers.
If you are planning to do this in a hot climate, please be aware that this mixture will heat up during the day. Lorne is in Arizona and found that temperatures in excess of 100F (38C) and beyond were encountered, which caused some warping and distortion of large pieces. If this is the case where you live, always add the component to a cold mixture and check the temperature during the day.
We will add to this original post in the thread as we learn more. If you wish to read the original Part 1 thread, it's here:-
link
Does it work? Hell yeah!! Here's a picture of a Commodore 64 case that I treated in eight hours. I only treated half of the case as a demonstration of how bad a case could be and yet it could still be restored.
Cheers
Merlin